COMPARISON OF NANOINDENTATION TESTERS IN TAIWAN

Yi-Ching Lin, Ya-Ko Chih

Abstract

The Center for Measurement Standards provides two test pieces for this exercise to compare a set of common data including elastic modulus and indentation hardness. Participating laboratories will perform the common test items on their systems and follow the recommended instructions. The distribution chart compiled from the experiment data provided by each laboratory can then be used to fully demonstrate the current state of nanoindentation testers. The experimentation method shall take the testing capabilities of each laboratory into consideration, and a full analysis shall be provided. The providers of experiment data shall be represented by an index code in the report. By participating in this comparison exercise, participants will be able to understand the differences and similarities between their own results and those of other laboratories; thus the results can be used as a reference basis for evaluation of the participant's testing capabilities.

Keywords
nanoindentation, elastic modulus, hardness
Download
IMEKO-TC5-2010-019.pdf
DOI
-
IMEKO TC
TC5 - Hardness Measurement

Event details

Event
HARDMEKO 2010
Technical Committee
TC5
Place
Pattaya, THAILAND
Time
21 November 2010 - 25 November 2010
Website
http://imeko2010.nimt.or.th/

Back to the proceedings