Skip to main content

DEVELOPMENT OF VISCO-ELASTO-PLASTIC MATERIAL MODEL FOR HUMAN TRABECULAR BONE USING NANOINDENTATION

Petr Zlámal, Ondřej Jiroušek, Daniel Kytýř, Jiří Němeček

Abstract

Knowledge of trabecular bone behaviour under loading is very important for bone quality assessment. For numerical modelling of deformation behaviour of trabecular tissue it is necessary to establish a material model for single trabeculae. For visco-elasto-plastic material model used in this study have to determine eight material constants. Two elastic constants were obtained directly from nanoindentation test by Oliver-Pharr method. Remaining material constants were identified from a Finite Element (FE) simulation of nanoindentation test.

Download
IMEKO-YSESM-2011-ea49.pdf
DOI
-
IMEKO TC
TC15 - Experimental Mechanics

Event details

Event
TC15 Youth Symposium 2011
Technical Committee
TC15
Place
Chemnitz, GERMANY
Time
25 May 2011 - 28 May 2011

Back to the proceedings