Abstract

Failure Mode and Effects Analysis (FMEA) is a procedure that is often skipped or not completed generally because of time of financial constraints, despite its proper use during the different steps of the product life cycle (design, development, manufacturing and maintenance) makes it possible to identify and possibly solve potentially critical problems. The most often skipped part of the FMEA procedure is that related to the sensing and measuring equipment, when present. Even when they are considered, the analysis is confined to the possible effects of failures that make them unavailable, while also the deviation from the expected metrological performance (larger uncertainty, as well as unexpected bias) may cause severe malfunctions in the whole system. This paper proposes a possible way to consider also the metrological performance of the sensing elements in the FMEA analysis and shows, also with a practical example, how they can be taken into account.

Keywords
FMEA, Measurement uncertainty, Target uncertainty, Errors, Failures
Download
IMEKO-TC10-2020-040.pdf
DOI
-
IMEKO TC
TC10 - Measurement for Diagnostics, Optimization and Control

Event details

Event
TC10 Conference 2020 (ONLINE)
Technical Committee
TC10
Email
viharos.zsolt@sztaki.mta.hu
Place
Dubrovnik, CROATIA
Time
20 October 2020 - 22 October 2020
Website
https://www.imekotc10-2020.com/
Proceedings
https://www.imeko.org/publications/tc10-2020

Back to the proceedings