NECESSITY OF RUSSIAN NANOINDENTATION STANDARD BASE DEVELOPMENT

Edward Aslanyan, Peter Krasowski
Abstract:
Over the past years a large number of papers have been published on the application of the nanoindentation method. These works describe various aspects of the nanoindentation method and provide a detailed overview of the characteristics of different hardware and software tools implementing this method. However, measurements taken under the same conditions and on the seemingly same samples often provide a significant discrepancy in the results on different instruments functioning according to the same principle. This paper discusses the issues of metrological support for the nanoindentation method in Russia.
Keywords:
nanoindentation method, Martens hardness, primary standard machine
Download:
IMEKO-TC5-2010-015.pdf
DOI:
-
Event details
IMEKO TC:
TC5
Event name:
HARDMEKO 2010
Title:
11th HARDMEKO Conference: HARDMEKO 2010 (together with 21st TC3 Conference on Measurement of Force, Mass and Torque and 2nd TC22 Meeting on Vibration Measurement)
Place:
Pattaya, THAILAND
Time:
21 November 2010 - 25 November 2010